In this paper, CaCO3, CoO, CuO as raw materials, using solid phase preparation of Ca3Co4O9-based thermoelectric materials doping Cu. The Ca3Co4O9-based thermoelectric material intermediates were prepared according to the stoichiometric ratio x=0.01, and the sintered crystals were prepared by using muffle furnace under different temperature setting conditions. X-ray diffraction (XRD) and Scanning electron microscopy (SEM) were used to analyze the crystallinity and morphology of the samples after sintering. The results show that the crystallinity of Ca3Co4O9-based thermoelectric materials is best when sintered at 800-850°C, and the crystallinity of samples sintered at 850°C is better than that at 800°C, The diffraction intensity ratio is stronger than 800°C. Continue to raise the temperature, Ca3Co4O9-based thermoelectric materials phase transition to Ca3Co2O6-based thermoelectric materials, When the sintering temperature is 1000°C, the product is Cu-doped Ca3Co2O6-based thermoelectric materials.

Full Text
Paper version not known

Talk to us

Join us for a 30 min session where you can share your feedback and ask us any queries you have

Schedule a call

Disclaimer: All third-party content on this website/platform is and will remain the property of their respective owners and is provided on "as is" basis without any warranties, express or implied. Use of third-party content does not indicate any affiliation, sponsorship with or endorsement by them. Any references to third-party content is to identify the corresponding services and shall be considered fair use under The CopyrightLaw.