Abstract

The YBCO films were directly deposited on the {1 1 0} 〈0 1 1〉 textured Ag substrates by ultrasonic spray pyrolysis method. The observed white points in YBCO film by one-step deposition at 900 °C consisted in high content of Ag on the surface of this film, which was due to the evaporation and diffusion of Ag atoms at high deposition temperature. While the performance of YBCO films was significantly enhanced using two-step deposition route. A 15 cm length of coated YBCO film on {1 1 0} 〈0 1 1〉 textured Ag tape was prepared by this two-step deposition method, which exhibited a transport J c value of more than 10 4 A/cm 2 (at 77 K).

Full Text
Paper version not known

Talk to us

Join us for a 30 min session where you can share your feedback and ask us any queries you have

Schedule a call

Disclaimer: All third-party content on this website/platform is and will remain the property of their respective owners and is provided on "as is" basis without any warranties, express or implied. Use of third-party content does not indicate any affiliation, sponsorship with or endorsement by them. Any references to third-party content is to identify the corresponding services and shall be considered fair use under The CopyrightLaw.