Abstract

Many obstacles impede the development of Li-air batteries for practical applications. In particular, there is lack of understanding of the dynamics of processes occurring in porous air electrodes during discharge, including oxygen transport limitations, pore clogging and electrode passivation by both insulating discharge and parasitic reaction products. Here, using small-angle neutron scattering, which provides information on the whole electrode adequate to electrochemical data, we uncover the mechanisms limiting the Li-O2 porous carbon electrode capacity by analysis of the cathode pore filling in highly and poorly solvating media - dimethyl sulfoxide and acetonitrile. The results obtained allowed us suppose that in both cases the cell death is mainly triggered by blocking of oxygen transport pathways inside carbon black particle agglomerates. Total discharge capacities are, indeed, higher in highly solvating solutions due to a higher discharge intermediate lifetime and longer diffusion distance, which enable Li2O2 formation outside the carbon black agglomerates, which are, as we demonstrated, in fact mesocrystals that are confirmed by the appearance of a diffraction peak in scattering curves.

Full Text
Paper version not known

Talk to us

Join us for a 30 min session where you can share your feedback and ask us any queries you have

Schedule a call

Disclaimer: All third-party content on this website/platform is and will remain the property of their respective owners and is provided on "as is" basis without any warranties, express or implied. Use of third-party content does not indicate any affiliation, sponsorship with or endorsement by them. Any references to third-party content is to identify the corresponding services and shall be considered fair use under The CopyrightLaw.