AbstractThe initial growth of Co thin films during plasma‐enhanced atomic layer deposition (PE‐ALD) is investigated by atomic force microscopy (AFM), scanning electron microscopy (SEM), and synchrotron radiation X‐ray reflectivity (SR‐XRR). For the PE‐ALD of Co, CoCp2 and NH3 plasma were used as precursor and reactant, respectively. From XRR simulation, the growth rate at the initial stage of growth did not linearly increase with growth cycles, showing deviation from ideal ALD growth. The low density of PE‐ALD‐produced Co film up to 100 cycles is observed from XRR and confirmed by AFM and SEM results. The growth behavior of Co is explained by island growth under substrate‐inhibited growth mode.

Full Text
Paper version not known

Talk to us

Join us for a 30 min session where you can share your feedback and ask us any queries you have

Schedule a call

Disclaimer: All third-party content on this website/platform is and will remain the property of their respective owners and is provided on "as is" basis without any warranties, express or implied. Use of third-party content does not indicate any affiliation, sponsorship with or endorsement by them. Any references to third-party content is to identify the corresponding services and shall be considered fair use under The CopyrightLaw.