Abstract
Through methods, such as microscope analysis, chemical analysis, metallography examination and scanning electron microscope etc, the causes resulting in high temperature reheater tube cracking of station boiler have been analyzed. The result indicates the crack is reheat crack, and structure stress, higher hardness and excessive welding residual stress are the primary inducement of tube joint crack.
Talk to us
Join us for a 30 min session where you can share your feedback and ask us any queries you have
Disclaimer: All third-party content on this website/platform is and will remain the property of their respective owners and is provided on "as is" basis without any warranties, express or implied. Use of third-party content does not indicate any affiliation, sponsorship with or endorsement by them. Any references to third-party content is to identify the corresponding services and shall be considered fair use under The CopyrightLaw.