Abstract
Direct current conductance in Al/(Al2O3)X(TiO2)1-X/silicon structure was studied, the dielectric layers being deposited by the chemical solution deposition method. The measurements were carried out at room temperature and 320, 340 and 360 K. The results correspond to bulk-limited conduction of the Poole-Frenkel type. High voltages and temperature lead to an additional current rise, explained by thermal excitation and tunneling of electrons through the lowered Poole-Frenkel barrier.
Talk to us
Join us for a 30 min session where you can share your feedback and ask us any queries you have
Disclaimer: All third-party content on this website/platform is and will remain the property of their respective owners and is provided on "as is" basis without any warranties, express or implied. Use of third-party content does not indicate any affiliation, sponsorship with or endorsement by them. Any references to third-party content is to identify the corresponding services and shall be considered fair use under The CopyrightLaw.