The effect of the heat treatment temperature on the physical properties of sol-gel silicon dioxide films derived from film-forming solutions is investigated experimentally. The dependencies of the thickness of the films, their refractive index, electrical strength, resistivity, etching rate, and the level of internal mechanical stresses on the treatment temperatures in the range from 700 to 1150 °C are obtained. It was found that the dependencies of the electrical strength, the etching rate, and the level of internal mechanical stresses have the sections with the different characters. The transition region between these sections corresponds to the heat treatment temperature equal to 900-950 °C.