Abstract

The hydrogen storage properties and microstructure of (V 30Ti 35Cr 25Fe 10) 1− x Si x ( x = 0–2.5 at.%) alloys were studied in this paper by PCT measurement, XRD and SEM/EDS. Laves phase appears in all Si-containing alloys ( x ≥ 0.32 at.%) except for BCC main phase, and the activation property is improved obviously by the occurring of Laves phase. The hydrogen absorption and desorption capacities decrease and the plateau pressures increase with the increase of Si content. Si exists mainly in Laves phase. The decrease of lattice parameter and the occurring of Laves phase by adding Si are the main reasons for the change of the hydrogen storage properties of the Si-containing alloys.

Full Text
Paper version not known

Talk to us

Join us for a 30 min session where you can share your feedback and ask us any queries you have

Schedule a call

Disclaimer: All third-party content on this website/platform is and will remain the property of their respective owners and is provided on "as is" basis without any warranties, express or implied. Use of third-party content does not indicate any affiliation, sponsorship with or endorsement by them. Any references to third-party content is to identify the corresponding services and shall be considered fair use under The CopyrightLaw.