The high-pressure sintering process is studied for the fabrication of the bulk CoSb 3 thermoelectric material. The CoSb 3 powder is prepared by a solid reaction method, and then the samples are sintered under high-pressure conditions. The emphasis of the present study is on the influence of the pressure on the grain size and the electrical properties of the material. For the present study, the pressure is taken to be from 1.5 GPa to 6 GPa, and the sintering temperature is 723 K. The experimental results show that the major phase of skutterudite and traces of metal impurities of Sb and the CoSb 2 phase coexist in some of the samples, and that the grain size of all the samples increase after sintering. In the range of 3.0 GPa to 6.0 GPa, the grain size increases with increasing pressure. In the range of 1.5 GPa to 3.0 GPa, the grain size also increases, but with a diminishing growth rate. All the materials show p-type transport behaviors, and the sample sintered under 2.0 GPa shows higher electrical conductivity than the 5.7 GPa sample, which may be due to the impurities.

Full Text
Paper version not known

Talk to us

Join us for a 30 min session where you can share your feedback and ask us any queries you have

Schedule a call

Disclaimer: All third-party content on this website/platform is and will remain the property of their respective owners and is provided on "as is" basis without any warranties, express or implied. Use of third-party content does not indicate any affiliation, sponsorship with or endorsement by them. Any references to third-party content is to identify the corresponding services and shall be considered fair use under The CopyrightLaw.