Abstract

Al-doped ZnO (AZO) thin films were potentiostatically deposited on indium tin oxide substrates. The influence of the doping level of the ZnO:Al films was investigated. The results of the X-ray diffraction and scanning electron microscopy analysis revealed that the structural properties of the AZO films were found polycrystalline with a hexagonal wurtzite-type structure along the (002) plane. The grain size of the AZO films was observed as approximately 3 μm in the film doping with 4 mol% ZnO:Al concentration. The thin films also exhibited an optical transmittance as high as 90 % in the wavelength range of 100–1,000 nm. The optical band gap increased from 3.33 to 3.45 eV. Based on the Hall studies, the lowest resistivity (4.78 × 10−3 Ω cm) was observed in the film doping with 3 mol% ZnO:Al concentration. The sheet resistant, carrier concentration and Hall mobility values were found as 10.78 Ω/ square, 9.03 × 1018 cm−3 and 22.01 cm2/v s, respectively, which showed improvements in the properties of AZO thin films. The ZnO:Al thin films were used as a buffer layer in thin-film solar cells with the structure of soda-lime glass/Mo/Cu2ZnSnS4/ZnS/ZnO/Al grid. The best solar cell efficiency was 2.3 % with V OC of 0.430 V, J SC of 8.24 mA cm−2 and FF of 68.1 %.

Highlights

  • Transparent conductive oxides (TCOs) have several applications and used in solar cells and solar thermal applications due to their wide band gap (Jager et al 1998; Qiao et al 2006)

  • Al-doped Zinc oxide (ZnO) (AZO) thin films were potentiostatically deposited on indium tin oxide substrates

  • The results of the X-ray diffraction and scanning electron microscopy analysis revealed that the structural properties of the AZO films were found polycrystalline with a hexagonal wurtzite-type structure along the (002) plane

Read more

Summary

Introduction

Transparent conductive oxides (TCOs) have several applications and used in solar cells and solar thermal applications due to their wide band gap (Jager et al 1998; Qiao et al 2006). The grain size of the AZO films was observed as approximately 3 lm in the film doping with 4 mol% ZnO:Al concentration. Based on the Hall studies, the lowest resistivity (4.78 9 10-3 X cm) was observed in the film doping with 3 mol% ZnO:Al concentration.

Results
Conclusion