Abstract
Thin films of La-doped hafnium oxide synthesized by plasma-enhanced atomic layer deposition with subsequent rapid annealing have been studied. It has been found that the films under study have an orthorhombic noncentrosymmetric structure with the space group Pmn21. It has been shown that these films have ferroelectric properties. The ratio of atomic concentrations of elements in a film has been determined. It has been found that the film consists of the mixture of the HfO2 and La2O3 phases. It has been shown that argon ion etching results in the generation of oxygen vacancies with a concentration of about 1 at % in the surface region of the films. Vacancies are formed primarily through the knock-out of oxygen atoms to interstitial positions with the formation of a Frenkel pair.
Talk to us
Join us for a 30 min session where you can share your feedback and ask us any queries you have
Disclaimer: All third-party content on this website/platform is and will remain the property of their respective owners and is provided on "as is" basis without any warranties, express or implied. Use of third-party content does not indicate any affiliation, sponsorship with or endorsement by them. Any references to third-party content is to identify the corresponding services and shall be considered fair use under The CopyrightLaw.