Abstract

Abstract Stress corrosion cracking (SCC) tests were carried out on specimens of Monel 400, Inconel 600, and Sanicro 30 steam generator tubing in solutions containing 10 to 500 g NaOH/kg H2O at 300 C for times up to 600 days. Applied stress and sodium hydroxide concentration had a significant effect on the (SCC) resistance of the three materials.

Talk to us

Join us for a 30 min session where you can share your feedback and ask us any queries you have

Schedule a call

Disclaimer: All third-party content on this website/platform is and will remain the property of their respective owners and is provided on "as is" basis without any warranties, express or implied. Use of third-party content does not indicate any affiliation, sponsorship with or endorsement by them. Any references to third-party content is to identify the corresponding services and shall be considered fair use under The CopyrightLaw.