Abstract
Silicon oxycarbide (SiOC) films on C/C composite substrate were prepared by isothermal chemical vapor deposition (CVD) with hexamethyldisilazane (HMDSN) as precursor. The deposition rate, microstructure, composition and mechanical properties of films prepared at deposition temperature ranging from 1300 K to 1576 K were investigated in details. With increasing deposition temperature, deposition rate increased gradually and reached a maximum value of 42.9 μm/h at 1513 K and then decreased; concurrently, the surface morphology of SiOC film changed from a smooth-dense to a coarse cauliflower, and then into a needle-like granular morphology. The SiOC films were composed of dominant SiC and a few other phases at all temperatures. In addition, the contents of oxygen-enriched units SiO3C and SiO2 increased with deposition temperature due to redistribution reaction of Si–O and Si–C bonds and oxidation. SiOC films prepared at 1373 K showed the highest hardness and elastic modulus for 28.8 GPa and 234.2 GPa, respectively. SiOC films also contained small amounts of Si3N4 and SiCN at all conditions.
Talk to us
Join us for a 30 min session where you can share your feedback and ask us any queries you have
Disclaimer: All third-party content on this website/platform is and will remain the property of their respective owners and is provided on "as is" basis without any warranties, express or implied. Use of third-party content does not indicate any affiliation, sponsorship with or endorsement by them. Any references to third-party content is to identify the corresponding services and shall be considered fair use under The CopyrightLaw.