Abstract

This paper outlines a method of sequentially joining steel laminations together using a high strength brazed joint to produce laminated tools. Individual joints were produced by using a heated platen rather than a furnace. Lap shear test samples were used to evaluate the tensile strengths of bonded laminates. Two laminate gauges were tested, 0.8mm and 1.6mm. Ranging trials were undertaken to determine optimum time to produce the joint. Constants for the trials were platen temperature, laminate material, braze material, joint area and joining pressure. At optimum conditions, that is the least time taken for highest tensile strength, the 0.8mm laminate averaged a strength of 4.7kN in 120 seconds’ heating time and the 1.6mm laminate averaged 9.3kN in 210 seconds.

Full Text
Paper version not known

Talk to us

Join us for a 30 min session where you can share your feedback and ask us any queries you have

Schedule a call

Disclaimer: All third-party content on this website/platform is and will remain the property of their respective owners and is provided on "as is" basis without any warranties, express or implied. Use of third-party content does not indicate any affiliation, sponsorship with or endorsement by them. Any references to third-party content is to identify the corresponding services and shall be considered fair use under The CopyrightLaw.