This research was conducted on the method of recovering the lithium hydroxide and valuable metal from the NCA-based cathode active materials in the spent lithium-ion batteries. The recovery rate of lithium depends on the reaction temperature, retention time, reaction time during H2 reduction and solid-liquid ratio. Lithium hydroxide and valuable metals were recovered under each experimental condition, and the following optimal process conditions were determined based on the results of experiment. Based on the charging of 10g of NCA powder, the optimal process conditions were determined as follows: the reaction temperature of 700?; the retention time of 3hrs; and the H2 gas flowrate of 300cc/min; the leaching time of 1hr for water leaching; the solid-liquid ratio of the sample and distilled water at 1:30; the stirring speed of 300rpm at room temperature, and the recovery rate of 92.30% was achieved.

Full Text
Paper version not known

Talk to us

Join us for a 30 min session where you can share your feedback and ask us any queries you have

Schedule a call

Disclaimer: All third-party content on this website/platform is and will remain the property of their respective owners and is provided on "as is" basis without any warranties, express or implied. Use of third-party content does not indicate any affiliation, sponsorship with or endorsement by them. Any references to third-party content is to identify the corresponding services and shall be considered fair use under The CopyrightLaw.