Abstract

We report on hybrid light-emitting devices (HLEDs) based on CdSe/ZnS quantum dots in polymer matrices. Color purity of the HLED with a mixed matrix consisting of polyvinylcarbazole (PVK) and 2-(4-biphenylyl)-5-(4-tert-butylphenyl)-1,3,4-oxadiazole (PBD) improves with the increasing concentration of PBD. We attribute this improvement to the increased electron mobility of the matrix. By using an n-type cyano-containing polymer derived from 6-(3,6-dibromo-9H-carbazol-9-yl)hexanenitrile and tetraphenylsilane to replace PVK:PBD as the matrix, further pure red emission with Commission Internationale De L'Eclairage coordinates of (0.67, 0.33) and maximum external quantum efficiency of 2.51% has been achieved.

Full Text
Paper version not known

Talk to us

Join us for a 30 min session where you can share your feedback and ask us any queries you have

Schedule a call

Disclaimer: All third-party content on this website/platform is and will remain the property of their respective owners and is provided on "as is" basis without any warranties, express or implied. Use of third-party content does not indicate any affiliation, sponsorship with or endorsement by them. Any references to third-party content is to identify the corresponding services and shall be considered fair use under The CopyrightLaw.