Poly(hydroxyalkanoates) are biodegradable and biocompatible polymers suitable for tissue engineering. Fused deposition modeling (FDM) belongs to modern rapid prototyping techniques for the fabrication of scaffolds. In this work, poly(3-hydroxybutyrate (PHB), poly(3-hydroxybutyrate-co-3-hydroxyvalerate) (PHBV) and poly(3-hydroxybutyrate-co-3-hydroxyhexanoate) (PHBH) were tested for FDM. Thermal and rheological properties of industrial PHAs were compared with poly(lactic acid) (PLA), which is a biodegradable polymer commonly used for FDM. The massive decrease in viscosity and loss of molecular weight of PHB and PHBV precluded their use for FDM. On the other hand, the thermal stability of PHBH was comparable to that of PLA. PHBH scaffolds prepared by FDM exhibited excellent mechanical properties, no cytotoxicity and large proliferation of mouse embryonic fibroblast cells within 96 h. The hydrolytic degradation of PHBH and PLA scaffolds tested in synthetic gastric juice for 52 days confirmed a faster degradation of PHBH than PLA. The decrease in molecular weight confirmed the first-order kinetics with a slightly higher (0.0169 day−1) degradation rate constant for PHBH as compared to the value (0.0107 day−1) obtained for PLA. These results indicate that PHBH could be used to produce scaffolds by FDM with application in tissue engineering.

Full Text
Paper version not known

Talk to us

Join us for a 30 min session where you can share your feedback and ask us any queries you have

Schedule a call

Disclaimer: All third-party content on this website/platform is and will remain the property of their respective owners and is provided on "as is" basis without any warranties, express or implied. Use of third-party content does not indicate any affiliation, sponsorship with or endorsement by them. Any references to third-party content is to identify the corresponding services and shall be considered fair use under The CopyrightLaw.