0.82NBT-0.18ST and 0.85NBT-0.15ST thin films have been prepared on Si substrates by a modified metalorganic solution deposition process. To achieve films with better ferroelectric properties, three main items have been changed in the process. Then the crystal structures, surface microstructures, hysteresis loops, fatigue curves and capacitance-voltage curves of the films were measured. It can be found that NBT-ST films can crystallize well after annealing at 650 °C for 5 minutes and have smooth surface microstructures. The 0.85NBT-0.15ST thin films exhibit better well-defined hysteresis loops than 0.82NBT-0.18ST, with a remnant polarization of 1.1 mC/cm2 and a coercive fields of 44.2 kV/cm. The clockwise C-V curves show that they have a desired polarization-type switching mode. The memory window of 0.82NBT-0.18ST thin film is about 1.8V, and that of 0.85NBT-0.15ST thin film is about 2.5V.

Talk to us

Join us for a 30 min session where you can share your feedback and ask us any queries you have

Schedule a call

Disclaimer: All third-party content on this website/platform is and will remain the property of their respective owners and is provided on "as is" basis without any warranties, express or implied. Use of third-party content does not indicate any affiliation, sponsorship with or endorsement by them. Any references to third-party content is to identify the corresponding services and shall be considered fair use under The CopyrightLaw.