Abstract

Natural diamond crystals with a highly porous surface were used as substrates for synthesizing single-phase bimetallic Pt–Co nanoparticles at temperatures of 500 °C and 800 °C. The metal nanoparticles inside the pores were determined to take the form of single-phase Pt0.50Co0.50 solid solutions with different degrees of superstructure ordering. A detailed characterization of both nanoalloys revealed a tetragonal symmetry with a space group, P4/mmm. For the sample obtained at 500 °C, the lattice parameters were a = 2.673(2), c = 3.735(3) Å, and c/a = 1.397(1); for the samples obtained at 800 °C, the parameters were—a = 2.688(2), c = 3.697(3) Å, and c/a = 1.375(1). Within the experimental parameters, no significant chemical interaction of the diamond with the Pt–Co particles was identified. The results demonstrate a strong anchoring effect of the metallic material within the etching pores. The successful synthesis of bimetallic Pt–Co particles embedded inside the caverns can facilitate a study of their magnetic properties. The presence of Pt–Co in specific diamond compositions can also be used for marking diamond crystals as a means for their subtle identification, as well as confirming the possibility of capturing significant amounts of metal along with diamonds during their dissolution in the deep Earth.

Full Text
Paper version not known

Talk to us

Join us for a 30 min session where you can share your feedback and ask us any queries you have

Schedule a call

Disclaimer: All third-party content on this website/platform is and will remain the property of their respective owners and is provided on "as is" basis without any warranties, express or implied. Use of third-party content does not indicate any affiliation, sponsorship with or endorsement by them. Any references to third-party content is to identify the corresponding services and shall be considered fair use under The CopyrightLaw.