Abstract

Taguchi’s method was applied to investigate the effect of the main HEBM parameters: milling time (MT), ball to powder weight ratio (BPWR) and milling speed (MS) on the dissolved AlN fraction in TiN. The settings of HEBM parameters were determined by using the orthogonal experiments array (OA). The as-received and milled powders were characterized by X-ray diffraction (XRD). The optimum milling parameter combination was determined by using the analysis of signal-to-noise (S/N) ratio. According to the analysis of variance (ANOVA) the milling speed is the most effective parameter and the optimal conditions for powder synthesis are: MT 20h, MS 600rpm, BPWR 50:1. The result of the experiment conducted under optimal conditions (AlN was completely dissolved during experiment) confirmed the conclusions of the statistical analysis.

Talk to us

Join us for a 30 min session where you can share your feedback and ask us any queries you have

Schedule a call

Disclaimer: All third-party content on this website/platform is and will remain the property of their respective owners and is provided on "as is" basis without any warranties, express or implied. Use of third-party content does not indicate any affiliation, sponsorship with or endorsement by them. Any references to third-party content is to identify the corresponding services and shall be considered fair use under The CopyrightLaw.