Abstract

In this paper we report on the formation of nickel silicide by electroless process. The nickel plating solution was composed of a mixture of NiSO 4·6H 2O, NaH 2PO 2·H 2O, Na 3C 6H 5O 7, and NH 4Cl, where NiSO 4·6H 2O is the main nickel source and NaH 2PO 2·H 2O is the reducing agent. The nickel silicide formation was carried out by heating the deposited samples in vacuum at temperatures from 100 °C to 800 °C. The evolution of NiSi phase from the nickel film was verified using the X-ray diffraction technique and Raman spectroscopy. The surface morphology was studied using AFM technique. The electroless plating technique can provide a cheap and easy process for forming nickel silicide, and has potentiality of application for the electronic device industries.

Talk to us

Join us for a 30 min session where you can share your feedback and ask us any queries you have

Schedule a call

Disclaimer: All third-party content on this website/platform is and will remain the property of their respective owners and is provided on "as is" basis without any warranties, express or implied. Use of third-party content does not indicate any affiliation, sponsorship with or endorsement by them. Any references to third-party content is to identify the corresponding services and shall be considered fair use under The CopyrightLaw.