Abstract

Two synthesis routes for approximately 100nm thick layers of LaNi0.6Fe0.4O3-δ (LNF64) are presented. Aqueous solutions of acetate or nitrate-precursors were deposited on Ce0.9Gd0.1O2-δ substrates by spin coating. After thermal annealing at 700°C for 3h, the thin films were characterized by X-ray diffraction, scanning electron microscopy, and X-ray photoelectron spectroscopy. The DC electrical conductivity of the LNF64 thin films was determined by four-point van der Pauw measurements as a function of temperature (20≤T/°C≤400) at 1×10−3≤pO2/bar≤1. At the surface and cross section a nanocrystalline microstructure with grain sizes of approximately 50–100nm was observed. The DC electrical conductivity of the thin films increases with increasing temperature and increasing pO2. A maximum electrical conductivity of 320S/cm was found at 400°C and pO2=1bar which agrees with the literature data for LNF64 bulk samples.

Talk to us

Join us for a 30 min session where you can share your feedback and ask us any queries you have

Schedule a call

Disclaimer: All third-party content on this website/platform is and will remain the property of their respective owners and is provided on "as is" basis without any warranties, express or implied. Use of third-party content does not indicate any affiliation, sponsorship with or endorsement by them. Any references to third-party content is to identify the corresponding services and shall be considered fair use under The CopyrightLaw.