Abstract

Mean hyperfine field H and isomer shifts I S obtained from Mössbauer measurements for rf sputtered (SP) and liquid quenched (LQ) Fe 1 − x B x (0.12 ⩽ x ⩽ 0.60 for SP and 0.13 ⩽ x ⩽ 0.24 for LQ) samples are compared with values for crystalline α-Fe, Fe 3B, Fe 2B and FeB. H and IS for both kinds of samples are in good agreement with those for the crystalline phases up to x ∼ 0.35. For SP films we observe a deviation from this tendency above x > 0.35. It seems that this effect is caused by chemical inhomogeneities in our films.

Full Text
Paper version not known

Talk to us

Join us for a 30 min session where you can share your feedback and ask us any queries you have

Schedule a call

Disclaimer: All third-party content on this website/platform is and will remain the property of their respective owners and is provided on "as is" basis without any warranties, express or implied. Use of third-party content does not indicate any affiliation, sponsorship with or endorsement by them. Any references to third-party content is to identify the corresponding services and shall be considered fair use under The CopyrightLaw.