Abstract

The substances involved in the sulfur-iodine (SI) thermochemical cycle to produce H2 by water splitting are very corrosive and may attack reactors, pumps, catalysts supports, and whatever part of the plant. This paper investigates the corrosion exerted by HI solutions in liquid, boiling, and gaseous phase at different temperatures. It shows the broadest overview of the behavior of different materials, ranging from pure metals to metallic alloys, from carbon materials to organic polymers, from ceramic materials to composite ones. Commercial nickel alloys and the effect of a specific element in their composition have here considerable attention. Regarding the composites materials, the impact of the substrate as well as the coating nature and thickness is studied, also through SEM-EDS (Scan Electron Microscope Energy Dispersive Spectroscopy) investigations.Carbon materials performed well, while most of the analyzed materials showed intergranular corrosion, pitting phenomena, and sometimes, carbide precipitation in the higher energy zones.

Talk to us

Join us for a 30 min session where you can share your feedback and ask us any queries you have

Schedule a call

Disclaimer: All third-party content on this website/platform is and will remain the property of their respective owners and is provided on "as is" basis without any warranties, express or implied. Use of third-party content does not indicate any affiliation, sponsorship with or endorsement by them. Any references to third-party content is to identify the corresponding services and shall be considered fair use under The CopyrightLaw.