Abstract

Magnetization measurements have been carried out on the magnetic shape memory alloys (MSMAs) Ni2Mn1.44−xCuxSn0.56 (0⩽x⩽0.09). On the basis of the experimental results, the phase diagram of Ni2Mn1.44−xCuxSn0.56 (0⩽x⩽0.09) alloys in the temperature-concentration plane has been determined. The resultant phase diagram is spanned by paramagnetic austenite (Para-A), ferromagnetic austenite (Ferro-A) and ferromagnetic martensite (Ferro-M) phases. The martensitic transition temperature TM makes a broad maximum as a function of x, whereas, in the austenite phase the Curie temperature TC decreases slightly with x. The TC of Ni2Mn1.415Cu0.025Sn0.56 was found to decrease linearly with pressure, whereas TM increased linearly with pressure. The values of dTM/dp and dTC/dp of Ni2Mn1.415Cu0.025Sn0.56 were found to be 0.88K/kbar and −0.31K/kbar, respectively.

Full Text
Paper version not known

Talk to us

Join us for a 30 min session where you can share your feedback and ask us any queries you have

Schedule a call

Disclaimer: All third-party content on this website/platform is and will remain the property of their respective owners and is provided on "as is" basis without any warranties, express or implied. Use of third-party content does not indicate any affiliation, sponsorship with or endorsement by them. Any references to third-party content is to identify the corresponding services and shall be considered fair use under The CopyrightLaw.