Abstract

On the grounds of theoretical results referred earlier formulae for the magnetic permeability dis-accomodation in dilute α-FeC type alloys containing substitutional (s) atoms are derived. In the calculations it is assumed that there is a strong repulsion of the interstitial (i) atom in the first coordination sphere of octahedral interstices of the s atom, attraction of the i atom in the second coordination sphere, lowering of the top of the energetical barrier for jumps of the i atom from the second to the third coordination sphere, and unchanged energetical barriers for other jumps. The results obtained are consistent with experimental data referred for α-Fe–V–C alloys, for which one additional relaxation placed at temperatures lower than the peak of the isochronal Snoek relaxation is found. Auf Grund von theoretischen Ergebnisen werden Formeln abgeleitet, die die Desakkommodation in α-Fe–C-Legierungen, die substitutionelle s-Atome enthalten, beschreiben. Es wird angenommen, das in der ersten Koordinationssphare der Oktaederlucken des s-Atoms die s- und die interstitiellen i-Atome sich stark gegenseitig abstosen, wahrend in der zweiten Sphare eine si-Anziehung zur Wirkung kommt. Es wird auch angenommen, das die energetischen Barrieren fur den Platzwechsel des i-Atoms zwischen der zweiten und dritten Sphare ein wenig niedriger liegen als zwischen normalen Lucken, die nur durch Eisenatome umgeben sind; fur Platzwechsel zwischen weiteren Spharen werden normale Barrieren eingefuhrt. Die erhaltenen Ergebnisse stimmen gut uberein mit den experimentellen Resultaten, die fur α-Fe–V–C Legierungen erhalten werden: fur diese Legierungen wird eine zusatzliche Relaxation, die bei tieferen Temperaturen erscheint als das Maximum der isochronen Desakkommodationskurve der Snoek-Relaxation, beobachtet.

Full Text
Published version (Free)

Talk to us

Join us for a 30 min session where you can share your feedback and ask us any queries you have

Schedule a call