Abstract
Herein, the synthesis of vanadium sulfide (VxSy) by atomic layer deposition (ALD) based on the use of tetrakis(dimethylamino) vanadium (IV) and hydrogen sulfide is presented for the first time. The (ultra)thin films VxSy are synthesized in a wide range of temperatures (100–225 °C) and extensively characterized by different methods. The chemical composition of the VxSy (ultra)thin films reveals different vanadium oxidation states and sulfur‐based species. Extensive X‐ray photoelectron spectroscopy analysis studies the effect of different ALD parameters on the VxSy chemical composition. Encouraged by the rich chemistry properties of vanadium‐based compounds and based on the variable valences of vanadium, the electrochemical properties of ALD VxSy (ultra)thin films as electrode material for supercapacitors are further explored. Thereby, nanotubular composites are fabricated by coating TiO2 nanotube layers (TNTs) with different numbers of VxSy ALD cycles at low temperature (100 °C). Long‐term cycling tests reveal a gradual decline of electrochemical performance due to the progressive VxSy thin films dissolution under the experimental conditions. Nevertheless, VxSy‐coated TNTs exhibit significantly superior capacitance properties as compared to the blank counterparts. The enhanced capacitance properties exhibited are derived from the presence of chemically stable and electrochemically active S‐based species on the TNTs surface.
Talk to us
Join us for a 30 min session where you can share your feedback and ask us any queries you have
Disclaimer: All third-party content on this website/platform is and will remain the property of their respective owners and is provided on "as is" basis without any warranties, express or implied. Use of third-party content does not indicate any affiliation, sponsorship with or endorsement by them. Any references to third-party content is to identify the corresponding services and shall be considered fair use under The CopyrightLaw.