Amorphous silicon carbide films were deposited by RF sputtering technique using a SiC target. These films were annealed in dry oxygen ambient in the temperature range of 400–700°C. Subsequently the films were characterized using X-ray photoelectron spectroscopy (XPS) to investigate the chemical composition at each annealing temperature. XPS indicated that increasing the anneal temperature results in a decrease in SiC phase, and an increase in SiOx. Surface morphology of the oxidized films was characterized using atomic force microscope. Optical absorption studies indicated blue shifting effects as the annealing temperature was increased.

Full Text
Paper version not known

Talk to us

Join us for a 30 min session where you can share your feedback and ask us any queries you have

Schedule a call

Disclaimer: All third-party content on this website/platform is and will remain the property of their respective owners and is provided on "as is" basis without any warranties, express or implied. Use of third-party content does not indicate any affiliation, sponsorship with or endorsement by them. Any references to third-party content is to identify the corresponding services and shall be considered fair use under The CopyrightLaw.