Abstract
The present study deals with the effect of activating flux and surface oxidation on micro structure, micro hardness and tensile strength of Tungsten Inert Gas welded 304 austenitic stainless steel plates. The thickness of the plate of 6.5 mm is considered for the investigation. The Tungsten Inert Gas welding is performed with 2.4mm diameter conical electrode tip profile with the surface condition of the plate as natural, oxidized and coated with an activating flux. Results have shown that the microstructure and mechanical properties are greatly influenced by activating flux and surface condition of plate. A-TIG welded plates give highest tensile strength when compared to TIG welded plates. Vickers micro hardness value is maximum nearer to the weld center on the cross section of the A-TIG butt weld joint.
Talk to us
Join us for a 30 min session where you can share your feedback and ask us any queries you have
More From: International Review of Mechanical Engineering-IREME
Disclaimer: All third-party content on this website/platform is and will remain the property of their respective owners and is provided on "as is" basis without any warranties, express or implied. Use of third-party content does not indicate any affiliation, sponsorship with or endorsement by them. Any references to third-party content is to identify the corresponding services and shall be considered fair use under The CopyrightLaw.