Methyl vinyl silicone rubber (MVQ)/low-melting-point alloy (SnBi) composites were prepared by mechanical blending. The effect of SnBi content on the surface resistivity, volume resistivity, mechanical properties, and transparency of MVQ were investigated. The results showed that the surface resistivity, volume resistivity, tensile strength, and elongation at break of MVQ/SnBi composites were 1.6 × 1010 Ω, 2.2 × 1011 Ω cm, 8.2 MPa, and 612%, respectively by incorporation of 3 phr SnBi, showing better antistatic properties and mechanical properties. The effect of cyclic stretching temperature, strain, and number of cycles on the aspect ratio (length to diameter), electrical performance, and mechanical properties of MVQ/SnBi composites were also studied. The average aspect ratio of the alloy particles increased with increasing tensile temperature, strain, and cyclic times, resulting in a reduction in electrical resistivity. In addition, the antistatic mechanism of MVQ/SnBi composites was revealed.

Full Text
Paper version not known

Talk to us

Join us for a 30 min session where you can share your feedback and ask us any queries you have

Schedule a call

Disclaimer: All third-party content on this website/platform is and will remain the property of their respective owners and is provided on "as is" basis without any warranties, express or implied. Use of third-party content does not indicate any affiliation, sponsorship with or endorsement by them. Any references to third-party content is to identify the corresponding services and shall be considered fair use under The CopyrightLaw.