Abstract
High-cycle fatigue fracture mechanisms and fatigue stress prediction of nickel-based single-crystal superalloys
Published Version
Talk to us
Join us for a 30 min session where you can share your feedback and ask us any queries you have
https://doi.org/10.1016/j.engfailanal.2024.109166
Copy DOIJournal: Engineering Failure Analysis | Publication Date: Dec 1, 2024 |
High-cycle fatigue fracture mechanisms and fatigue stress prediction of nickel-based single-crystal superalloys
Join us for a 30 min session where you can share your feedback and ask us any queries you have
Disclaimer: All third-party content on this website/platform is and will remain the property of their respective owners and is provided on "as is" basis without any warranties, express or implied. Use of third-party content does not indicate any affiliation, sponsorship with or endorsement by them. Any references to third-party content is to identify the corresponding services and shall be considered fair use under The CopyrightLaw.