Abstract
The heat of formation, $\ensuremath{\Delta}H$, of metal hydrides is empirically found to be linearly related to a characteristic energy $\ensuremath{\Delta}E$ of the electronic band structure of the host metal. Independently of the position of the host metal in the Periodic Table (simple metals, noble metals, transition metals, actinides, and rare earths) we found $\ensuremath{\Delta}H=\ensuremath{\alpha} \ensuremath{\Delta}E+\ensuremath{\beta}$, with $\ensuremath{\Delta}E={E}_{F}\ensuremath{-}{E}_{s}$, $\ensuremath{\alpha}=29.62$ kJ/eV mol H, and $\ensuremath{\beta}=\ensuremath{-}135$ kJ/mol H (${E}_{F}$ is the Fermi energy and ${E}_{s}$ is the center of the lowest band of the host metal; $\ensuremath{\Delta}H$ is expressed in kJ/mol H and $\ensuremath{\Delta}E$ in eV). Assuming that this relation also holds for ternary metal hydrides we used the (simple) tight-binding coherent-potential-approximation model of Cyrot and Cyrot-Lackmann to evaluate the characteristic energy $\ensuremath{\Delta}E$ of ${A}_{{y}_{A}}{B}_{{y}_{B}}$ alloys where $A$ and $B$ are both nonsimple metals. The values of $\ensuremath{\Delta}H$ derived from the calculated $\ensuremath{\Delta}E$ are in good agreement with existing experimental data on the heat of formation of ternary metal hydrides.
Talk to us
Join us for a 30 min session where you can share your feedback and ask us any queries you have
Disclaimer: All third-party content on this website/platform is and will remain the property of their respective owners and is provided on "as is" basis without any warranties, express or implied. Use of third-party content does not indicate any affiliation, sponsorship with or endorsement by them. Any references to third-party content is to identify the corresponding services and shall be considered fair use under The CopyrightLaw.