Near-stoichiometric LiTaO 3 single crystals, 80 mm in diameter and 25–30 mm in length, were grown by conventional Czochralski technique using radio-frequency heating and automatic control system. Two compositions of the starting melt were used, containing accordingly 58 and 60.5 mol% Li 2O. The chemical composition of the grown crystals was estimated by measuring their coercive field to be 49.75–49.8 and 49.93–49.97 mol% Li 2O for these two starting melts.

Full Text
Paper version not known

Talk to us

Join us for a 30 min session where you can share your feedback and ask us any queries you have

Schedule a call

Disclaimer: All third-party content on this website/platform is and will remain the property of their respective owners and is provided on "as is" basis without any warranties, express or implied. Use of third-party content does not indicate any affiliation, sponsorship with or endorsement by them. Any references to third-party content is to identify the corresponding services and shall be considered fair use under The CopyrightLaw.