Thin aluminum oxide (Al 2O 3) films were grown by plasma-assisted atomic layer controlled deposition (PAALD) method using Dimethylethylamine alane ((CH 3) 2 (C 2H 5)N:AlH 3) (DMEAA). Al was deposited by PAALD method, then the Al films were oxidized into Al 2O 3 by the plasma oxidation in the same chamber without breaking the vacuum. Al 2O 3 thin films of 15 nm thickness were prepared by repetition of the above mentioned process. Thus, prepared Al 2O 3 thin films showed a refractive index of 1.68. The thickness and the refractive index fluctuation of the film over a 4-in. wafer were ±2.3% and ±1.9%, respectively, for atomic layer controlled deposited films. The leakage current density and breakdown field were measured to be about 10 −8 A/cm 2 at 1 and 7 MV/cm, respectively.
Talk to us
Join us for a 30 min session where you can share your feedback and ask us any queries you have
Disclaimer: All third-party content on this website/platform is and will remain the property of their respective owners and is provided on "as is" basis without any warranties, express or implied. Use of third-party content does not indicate any affiliation, sponsorship with or endorsement by them. Any references to third-party content is to identify the corresponding services and shall be considered fair use under The CopyrightLaw.