Abstract
This paper describes the fracture characteristics of both fibres and matrix in tensile, compressive and flexural failures of carbon fibre-reinforced PEEK composites and considers their relevance to the analysis of the failure of structures fabricated from such material.
Talk to us
Join us for a 30 min session where you can share your feedback and ask us any queries you have
Disclaimer: All third-party content on this website/platform is and will remain the property of their respective owners and is provided on "as is" basis without any warranties, express or implied. Use of third-party content does not indicate any affiliation, sponsorship with or endorsement by them. Any references to third-party content is to identify the corresponding services and shall be considered fair use under The CopyrightLaw.