Abstract

The fabrication of BaZrO3 (BZO) and La2Zr2O7 (LZO) films was investigated using metal-organic deposition with 2-ethylhexanates on substrates of LaAlO3(100) (LAO) single crystals and Ni-electroplated cube-textured Cu tapes. BZO and LZO films were grown epitaxially on LAO at temperatures above 600 and 750 °C in air, respectively. The BZO and LZO films on LAO had smooth surfaces with root mean square roughness of 1.4 and 0.4 nm, respectively. In contrast, BZO and LZO films fired on Ni/Cu substrates had polycrystalline structures with grain sizes of 10–20 nm.

Talk to us

Join us for a 30 min session where you can share your feedback and ask us any queries you have

Schedule a call

Disclaimer: All third-party content on this website/platform is and will remain the property of their respective owners and is provided on "as is" basis without any warranties, express or implied. Use of third-party content does not indicate any affiliation, sponsorship with or endorsement by them. Any references to third-party content is to identify the corresponding services and shall be considered fair use under The CopyrightLaw.