Lead-free (1–x)(Na0.5Bi0.5)0.7Sr0.3TiO3–xKNb0.6Ta0.4O3 ((1−x)NBST–xKNT, x = 0–0.3) ceramics were synthesized via citrate combustion process. The addition of KNT reduces the grain size, decreases the remanent polarization (P r), and slimmer hysteresis loops are realized. (1−x)NBST–xKNT ceramics exhibit typical relaxor characteristics as x increases. A large recoverable energy storage density (W re ∼ 1.74 J/cm3) and high efficiency (η ∼ 87%) are obtained for 0.8NBST–0.2KNT ceramic sample at 150 kV/cm. The energy-storage performances of 0.8NBST–0.2KNT sample show excellent temperature stability (W re varies 9.7% and η varies 2.3% within 25–75 °C).

Full Text
Paper version not known

Talk to us

Join us for a 30 min session where you can share your feedback and ask us any queries you have

Schedule a call

Disclaimer: All third-party content on this website/platform is and will remain the property of their respective owners and is provided on "as is" basis without any warranties, express or implied. Use of third-party content does not indicate any affiliation, sponsorship with or endorsement by them. Any references to third-party content is to identify the corresponding services and shall be considered fair use under The CopyrightLaw.