Using the microwave sintering technology, the effects of phosphorus (P) additions on the microstructure and properties of the ultrafine WC-10Co alloys were investigated. The experimental results show that with only 0.3wt% P additions, full density WC-10Co cermets were obtained at temperature of 1250 °C, which is 70 °C lower than that of the undoped counterparts. Lower sintering temperature can result in finer WC grain growth; therefore, the P-doped WC-10Co alloys exhibited higher hardness than the undoped ones. But at the same time, P doping could lead to sacrifice of fracture toughness of WC-10Co cemented carbides.
Talk to us
Join us for a 30 min session where you can share your feedback and ask us any queries you have
More From: Journal of Wuhan University of Technology-Mater. Sci. Ed.
Disclaimer: All third-party content on this website/platform is and will remain the property of their respective owners and is provided on "as is" basis without any warranties, express or implied. Use of third-party content does not indicate any affiliation, sponsorship with or endorsement by them. Any references to third-party content is to identify the corresponding services and shall be considered fair use under The CopyrightLaw.