Abstract
In this work, wet-process fibreboards (hardboards) were produced in the laboratory using industrial wood fibres of the species European beech (Fagus sylvatica L.) and Turkey oak (Quercus cerris L.) at the total volume of 40%, and white poplar (Populus alba L.) at 60% volume. The effects of hot pressing pressure (varied from 3.3 MPa to 5.3 MPa) and pressing time (from 255 s to 355 s) on the physical and mechanical properties of hardboards were investigated and optimal values of the parameters for fulfilling the European standard requirements were determined. It was concluded that hardboards with acceptable physical and mechanical properties may be produced from 60% poplar wood waste and residues, combined with 40% hardwood raw materials (beech and oak) by regulating the hot pressing regime only, i.e. pressure and pressing time. The following minimum parameters for producing hardboards from mixed hardwood tree species were determined: a pressure of 4.6 MPa and a pressing time of 280 s.
Talk to us
Join us for a 30 min session where you can share your feedback and ask us any queries you have
Disclaimer: All third-party content on this website/platform is and will remain the property of their respective owners and is provided on "as is" basis without any warranties, express or implied. Use of third-party content does not indicate any affiliation, sponsorship with or endorsement by them. Any references to third-party content is to identify the corresponding services and shall be considered fair use under The CopyrightLaw.