Abstract

The space charge region (SCR) width of the Schottky barrier (SB) that forms on the interface between aluminum and organic semiconductor polymer of bulk-heterojunction (BH) organic photodiodes (OPD) based on poly(3-hexylthiophene) (P3HT): [6,6]-phenyl-C61-butyric acid methylester (PCBM) blend, has been investigated according to reverse voltage bias over the OPD. We focused on the effect of incident light power (ILP) on the SCR and the I-V characteristics of the devices. Comparison of the mathematical models and experimental data measured under different ILPs indicate a dependency of SCR to the ILP.

Talk to us

Join us for a 30 min session where you can share your feedback and ask us any queries you have

Schedule a call

Disclaimer: All third-party content on this website/platform is and will remain the property of their respective owners and is provided on "as is" basis without any warranties, express or implied. Use of third-party content does not indicate any affiliation, sponsorship with or endorsement by them. Any references to third-party content is to identify the corresponding services and shall be considered fair use under The CopyrightLaw.