Abstract

Synthetic and totally amorphous styrene-butadiene rubber (SBR) has been loaded with varying contents of boric acid. Vulcanization of prepared composites as well as of unloaded rubber has been induced by ionizing radiation of accelerated electron beam of varying doses up to 250 kGy. Evaluation of prepared composite subjected to this range of irradiation has been followed up through the measurement of mechanical, physical, electrical and thermal properties of vulcanized composites. Mechanical properties, namely tensile strength (TS) and Young’s modulus were found to increase, whereas elongation at break ( E b) and permanent set (PS) were found to decrease with the increase in degree of boric acid loading as well as irradiation dose. On the other hand, physical properties, namely the gel content, have increased whereas the swelling number has decreased. Moreover, increase in the decomposition temperature has been attained. Also, limited increase in electrical conductivity has taken place. Data obtained indicate enhancement in thermal as well as in physico-mechanical properties of prepared composites. Moreover, 60 phr of boric acid has attained good mechanical properties.

Full Text
Paper version not known

Talk to us

Join us for a 30 min session where you can share your feedback and ask us any queries you have

Schedule a call

Disclaimer: All third-party content on this website/platform is and will remain the property of their respective owners and is provided on "as is" basis without any warranties, express or implied. Use of third-party content does not indicate any affiliation, sponsorship with or endorsement by them. Any references to third-party content is to identify the corresponding services and shall be considered fair use under The CopyrightLaw.