Abstract

The in-depth profiles of iron in silicon diffused with iron at 800, 900, 1000 and 1070°C were investigated by DLTS measurements. The diffusion coefficient of interstitial iron in silicon was represented by the expression DFe=9.5×10-4 exp (-0.65/kT) cm2s-1 in the temperature range of 800–1070°C.