Abstract

The grain‐growth behavior and grain‐boundary structure in titanium‐excess BaTiO3 depend on the amount of excess titanium at 1250° and 1300°3C. With excess titanium, abnormal grain growth (AGG) occurs and the grain boundaries are mostly flat or faceted with hill‐and‐valley shapes. With 0.5 at.% excess titanium, the large grains have flat {111} faces forming singular grain boundaries parallel to {111} double twins. With excess‐titanium content between 0.1 and 0.3 at.%, the abnormal grains appear to have polyhedral shapes with {100} faces. These flat or faceted grain boundaries are expected to have singular structures, and hence AGG can occur by the step growth mechanism. When the excess‐titanium content is decreased to 0, the grain boundaries become curved, indicating a rough atomic structure, and normal grain growth occurs.

Talk to us

Join us for a 30 min session where you can share your feedback and ask us any queries you have

Schedule a call

Disclaimer: All third-party content on this website/platform is and will remain the property of their respective owners and is provided on "as is" basis without any warranties, express or implied. Use of third-party content does not indicate any affiliation, sponsorship with or endorsement by them. Any references to third-party content is to identify the corresponding services and shall be considered fair use under The CopyrightLaw.