Abstract

AbstractDuring vitrification of radioactive wastes, excessive foaming reduces processing rates within melters by hindering heat transfer from the molten glass pool to the reacting melter feed. Formulations of low‐activity waste (LAW) melter feeds, for vitrification at the Waste Treatment and Immobilization Plant at the Hanford Site, conventionally include the addition of sucrose to mitigate excessive foaming by hastening the denitration process. However, incomplete combustion of sucrose produces organics such as acetonitrile (C2H3N) that may exceed bounding limits of downstream effluent treatment facilities. Using boron nitride (BN) as an alternate reductant to sucrose, in a representative LAW melter feed reduced C2H3N production by 90% by preventing the low‐temperature sucrose–nitrate reactions. Furthermore, foaming was suppressed due to the higher decomposition temperature of BN than H3BO3 meaning a delayed reaction of a large fraction of boron with the transient glass‐forming melt until above the foam onset temperature, thus reducing the quantity and viscosity of the connected melt and trapping less gas in the foam layer.

Talk to us

Join us for a 30 min session where you can share your feedback and ask us any queries you have

Schedule a call

Disclaimer: All third-party content on this website/platform is and will remain the property of their respective owners and is provided on "as is" basis without any warranties, express or implied. Use of third-party content does not indicate any affiliation, sponsorship with or endorsement by them. Any references to third-party content is to identify the corresponding services and shall be considered fair use under The CopyrightLaw.