AbstractHere we report a new atomic layer deposition (ALD) process for WO3 thin films based on W(CO)6 as a tungsten source and ozone as a source of oxygen. A narrow ALD temperature window is found at 195–205 °C for WO3 with a deposition rate of 0.23 Å per cycle. As‐deposited films are partially crystalline with root mean square (rms) roughness values of 4.7 nm for 90 nm thick films; annealing the films at 600–1000 °C under oxygen or nitrogen atmospheres enhances the degree of crystallinity considerably. Our results show that the straightforward ALD chemistry of carbonyl compounds and ozone is applicable to the deposition of WO3 thin films.

Talk to us

Join us for a 30 min session where you can share your feedback and ask us any queries you have

Schedule a call

Disclaimer: All third-party content on this website/platform is and will remain the property of their respective owners and is provided on "as is" basis without any warranties, express or implied. Use of third-party content does not indicate any affiliation, sponsorship with or endorsement by them. Any references to third-party content is to identify the corresponding services and shall be considered fair use under The CopyrightLaw.