Clean renewable energy sources (e.g., solar, wind, and hydro) offers the most promising solution to energy and environmental sustainability. On the other hand, owing to the spatial and temporal variations of renewable energy sources, and transportation and mobility needs, high density energy storage and efficient energy distribution to points of use is also critical. Moreover, it is challenging to scale up those processes in a cost-effective way. Electrochemical processes, including photoelectrochemical devices, batteries, fuel cells, super capacitors, and others, have shown promise for addressing many of the abovementioned challenges. Materials with designer properties, especially the interfacial properties, play critical role for the performance of those devices. Atomic layer deposition is capable of precise engineering material properties on atomic scale. In this review, we focus on the current state of knowledge of the applications, perspective and challenges of atomic layer deposition process on the electrochemical energy generation and storage devices and processes.
Talk to us
Join us for a 30 min session where you can share your feedback and ask us any queries you have
More From: Journal of Vacuum Science & Technology A: Vacuum, Surfaces, and Films
Disclaimer: All third-party content on this website/platform is and will remain the property of their respective owners and is provided on "as is" basis without any warranties, express or implied. Use of third-party content does not indicate any affiliation, sponsorship with or endorsement by them. Any references to third-party content is to identify the corresponding services and shall be considered fair use under The CopyrightLaw.