Abstract
The possibility of using technical nitrogen including 0,2% O2 for activation austenitic steels surfaces during gas nitriding were investigated. By changing mole fraction of technical nitrogen i NH3 /N2t mixture one can regulate oxygen potential of gas atmosphere during heating the steel to nitriding temperature and sometimes during nitriding process. Four representative austenitic steels were nitrided with good results at 570°C and under 450°C. New method can be alternative to regulating oxygen potential by air and allows avoiding installing of firing mechanism and safety control.