Abstract
To assess the strength and reliability of welded joints, the metal of welded joints of the unstable condensate pipeline was tested for static tension and low-cycle durability. The tests were carried out on defect-free specimens, specimens with defects such as lack of fusion, undercut, single pore, single slag inclusion and specimens with defects combining lack of fusion and undercut. A comparative analysis of the effect of defects combining lack of penetration and undercut and separately located defects such as lack of penetration, undercut, single pore, single slag inclusion on tensile strength and low-cycle durability of welded joints is carried out.