Abstract
Treatment of the stable N-heterocyclic carbene 1,3-di-tert-butylimidazolin-2-ylidene with 2 equiv of AlH3(NMe3) afforded the structurally unusual ring-expanded dialane complex 1 in 72% yield after ...