Micron-sized nanoporous silver powder with pore size of ∼100–160nm and specific surface area of ∼4.7–5.5m2/g was synthesized from three mechanically alloyed Ag-Zn powders (composition: 25, 50 and 75 at.% Zn). Dealloying was carried out at free corrosion conditions in NaOH, HCl and AgNO3 solutions. Both partial and complete dealloying were obtained by suitable choice of electrolyte and time of exposure. Zn in the solution after dealloying was recovered in the form of ZnO nanoparticles with particle size of 55.7±18nm. The effect of composition and electrolyte on the degree of dealloying was also studied.

Full Text
Paper version not known

Talk to us

Join us for a 30 min session where you can share your feedback and ask us any queries you have

Schedule a call

Disclaimer: All third-party content on this website/platform is and will remain the property of their respective owners and is provided on "as is" basis without any warranties, express or implied. Use of third-party content does not indicate any affiliation, sponsorship with or endorsement by them. Any references to third-party content is to identify the corresponding services and shall be considered fair use under The CopyrightLaw.